The effect of short-term (3- and 6-h-long) periodic thermal aging was investigated at three different temperatures on PVC cables and PVC films. Three different temperatures (110, 125, and 140 °C) were used for aging PVC cables and one (110 °C) for PVC films. PVC films were prepared for the investigation containing 0, 30, 40, and 50 weight percent of dioctyl phthalate plasticizer (DOP).