This study was to evaluate the effect of different water amounts and hydrolysis times of silane coupling agent on shear bond strength between lithium disilicate glass ceramic (LDS) and composite resin. Fourteen groups (n=7) of different water amounts (90, 50 and 10%v/v) and hydrolysis times (5, 19, 75 and 300 s) of experimental silane coupling agent that were prepared for silanization, non-silanization and commercial silane coupling agent (CSC) groups. Two-way analysis of variance (ANOVA) revealed no interaction between water amounts and hydrolysis times of ESC on shear bond strength between LDS and composite resin.
View Article and Find Full Text PDFObjectives: This study evaluated color differences (Δs) and translucency parameter changes (Δs) of various computer-aided design/computer-aided manufacturing (CAD/CAM) blocks after immersion in coffee.
Materials And Methods: Eight CAD/CAM blocks and four restorative composite resins were evaluated. The CIE values of 2.
This study investigated the surface roughness and gloss of composite resin CAD/CAM blocks after toothbrushing. Five composite resin blocks (Block HC, Cerasmart, Gradia Block, KZR-CAD Hybrid Resin Block, and Lava Ultimate), one hybrid ceramic (Vita Enamic), one feldspar ceramic (Vitablocs Mark II), one PMMA block (Telio CAD), and one conventional composite resin (Filtek Z350 XT) were evaluated. Surface roughness (Ra) and gloss were determined for each group of materials (n=6) after silicon carbide paper (P4000) grinding, 10k, 20k, and 40k toothbrushing cycles.
View Article and Find Full Text PDFUnlabelled: The aim of the study was to investigate two- and three-body wear of CAD/CAM blocks. Four composite resins, one hybrid ceramic and one feldspar ceramic block material were examined. Six specimens each were tested in a ball-on-disc wear device fitted with a zirconia ball (50 N load, 1.
View Article and Find Full Text PDFThis study compared commercial composite resin blocks with one ceramic block for use in computer-aided design/computer aided manufacturing (CAD/CAM). Four composite resins, one composite ceramic, and one feldspar-ceramic block were investigated. Flexural strength (FS), flexural modulus (FM), and Vickers hardness (VH) were determined under three conditions: dry storage; immersion in water at 37°C for 7 days; and immersion in water at 37°C for 7 days followed by 10,000 thermocycles.