The present article deals with the development of 3D porous scaffolds for bone grafting. They were prepared based on rapid fluid infiltration of Al2O3-SiO2 sol into a polyethylene non-woven fabric template structure. Titanium dioxide in concentration equal to 5 wt% was added to the Al2O3-SiO2 mixture to produce Al2O3-SiO2-TiO2 composite scaffolds.
View Article and Find Full Text PDFLaminated Si/SiC ceramics were synthesized from porous preforms of biogenous carbon impregnated with Si slurry at a temperature of 1500 °C for 2 h. Due to the capillarity infiltration with Si, both intrinsic micro- and macrostructure in the carbon preform were retained within the final ceramics. The SEM micrographs indicate that the final material exhibits a distinguished laminar structure with successive Si/SiC layers.