We report on a synthetic method where polyanhydride is used as starting material and the ester monomers are inserted through complete esterification, leading to an alternating ester-anhydride copolymer. The molar ratio of ricinoleic acid (RA) and sebacic acid (SA) was optimized until polysebacic acid is completely converted to carboxylic acid-terminated RA-SA and RA-SA-RA ester-dicarboxylic acids. These dimers and trimers were activated with acetic anhydride, polymerized under heat and vacuum to yield alternating RA-SA copolymer.
View Article and Find Full Text PDFPoly(anhydride) are unstable and prone to hydrolytic degradation and depolymerisation via anhydride interchange. They are stored at -20°C, packed under inert atmosphere until use. We synthesized a new poly(anhydride) from ricinoleic (RA) and sebacic (SA) acid with alternating ester-anhydride structure that is stable at 25°C for over 18months.
View Article and Find Full Text PDF