Artificially cemented sandstones were produced to assess the impact of detrital texture and composition on the precipitation and distribution of early calcite cement, and cement-related degradation in porosity. To simulate early-calcite cementation, loose sediment of variable composition (siliciclastic and calcareous) and grain size was exposed to a calcite supersaturated solution for 35 to 58 days at 23°C. Identification and distribution of the newly precipitated crystals was performed with high resolution 2D optical and scanning electron microscopy.