Corncob hull was immersed in 25 wt% H(2)SO(4) and was carbonized in an oven at 290 °C for 2h to obtain the char. The char was then activated for 1h at 780 °C by KOH at weight ratio of KOH/char of 2.5, 3.
View Article and Find Full Text PDFIn this work, unburnt coal (UC) in bottom ash from coal-fired power plants was soaked in KOH solution and activated for 1 h at 780 degrees C. The yield of activated carbons varied from 47.8 to 54.