Nickel laterites cannot be effectively used in physical methods because of their poor crystallinity and fine grain size. Na2SO4 is the most efficient additive for grade enrichment and Ni recovery. However, how Na2SO4 affects the selective reduction of laterite ores has not been clearly investigated.
View Article and Find Full Text PDF