Purpose: To evaluate the use of demineralized bone matrix of caprine origin in experimental bone defects of the tibia in New Zealand rabbits.
Methods: Fragments of the tibia diaphysis were collected aseptically from clinically healthy goats. The bones were sectioned into 1 cm fragments and stored at -20°C for subsequent hydrochloric acid (HCL) demineralization.