In most cases, stone mastic asphalt (SMA) mixtures placed in thin layers and subjected to stress develop early cracks (potentially resulting from being improperly affixed to the underlying layer, placed over previously cracked asphalt pavement, or placed over Portland cement concrete slabs). However, the filler used in SMA production is very influential on the performance of the mix. Fillers used in this type of mixture have a low plastic index or are inert (calcium carbonate or lime), so it is important to understand the effect of each material on the possible fissuring and cracking process of the SMA mixture.