Autoclave leaching of sulfide concentrates may produce various ferric secondary phases, depending on the arsenic content and temperature. Silver is converted to argentojarosite, from which it is not recoverable by standard cyanidation methods. To increase silver recovery, it is necessary to reduce the argentojarosite formation during autoclave leaching.
View Article and Find Full Text PDFThe research of this paper was carried out on the low-temperature (100 ± 2 °C) pressure (0.2-0.8 MPa) leaching of pyrite, chalcopyrite and their mixture.
View Article and Find Full Text PDFAn integrated two-stage metallurgical process has been developed to process concentrates from the Olimpiadinskoe deposit, which contain high levels of antimony and arsenic. The optimal parameters for the alkaline sulfide leaching process of the initial concentrate from the Olimpiadinskoe deposit were determined to achieve the maximum extraction of antimony at a 99% level. The recommended parameters include an L:S ratio of 4.
View Article and Find Full Text PDFThe nature of tennantite (Cu12As4S13), chalcopyrite (CuFeS2) and sphalerite (ZnS) particles’ mixture dissolution in nitric acid (HNO3) media was investigated in this study. The effects of temperature (323−368 K), HNO3 (1−8 mol/L) and Fe3+ (0.009−0.
View Article and Find Full Text PDFThis paper describes the nitric acid dissolution process of natural minerals such as tennantite, chalcopyrite and sphalerite, with the addition of Fe (III) ions and FeS. These minerals are typical for the ores of the Ural deposits. The effect of temperature, nitric acid concentration, time, additions of Fe (III) ions and FeS was studied.