Aim: To evaluate the shear bond strength of current luting cements to sandblasted crown-coping substrates.
Methods: Specimens of nickel-chromium, pressable glass ceramic, and zirconia crown-coping substrates were sandblasted in three groups (n = 30 each) with 50 (group 1), 110 (group 2), and 250 μm (group 3) alumina particles at a pressure of 250 kPa. Cylinders of glass ionomer, universal resin, and self-adhesive resin cements were then built up on the sandblasted substrate surfaces of each group (n = 10).