The objective of this study was to evaluate the effect of passive or active phosphoric acid (PA) application after hydrofluoric acid (HA) treatment on the microshear bond strength of lithium disilicate. Thirty ceramic discs were made with IPS Emax 2 (10 mm thick and 10 mm diameter). The specimens were divided into 3 groups, A: 9.