Fabricating large-scale porous bioactive glass bone scaffolds presents significant challenges. This study aims to develop formable, in situ setting scaffolds with a practical gelation time of about 10 min by mixing 45S5 bioactive glass with sodium silicate (waterglass) and an acid initiator. The effects of pH (2-11), waterglass concentration (15-50 wt.
View Article and Find Full Text PDFAdv Colloid Interface Sci
December 2023
Sodium silicate solutions, also known as waterglass, have been found to have remarkable utility in a variety of applications. The cumulative weight of evidence from 70 years of varied analysis indicates that silicate solutions consist of a wide range of species, from monomers through oligomers, up to colloids. Moreover, the structure and distribution of these species are greatly dependent upon many parameters, such as solute concentrations, silica to alkali ratio, pH, and temperature.
View Article and Find Full Text PDFBackground: Intrauterine growth factor (IUGR) is one of the most important causes of neonatal mortality. The aim of this study was to evaluate the therapeutic effect of utrogestan on the treatment of IUGR and its complications.
Materials And Methods: In this clinical trial, 66 pregnant women with idiopathic IUGR embryos were enrolled.
In this study porous scaffolds of chitosan (CS) and carboxymethyl cellulose (CMC) reinforced with whisker-like biphasic and triphasic calcium phosphate fibers were fabricated by freeze drying method. The effect of addition of CMC, fiber type and content on the mechanical, physicochemical and biological properties of the composite scaffolds was evaluated. The fibers were synthesized by homogenous precipitation method and were characterized.