Int J Prosthodont
August 2008
Purpose: The aim of this prospective study was to evaluate the clinical performance of fully sintered hot isostatic pressed yttria-partially-stabilized zirconia (Denzir) 3-unit fixed partial dentures (FPDs).
Materials And Methods: Nineteen 3-unit FPDs were placed in 18 patients. Ten FPDs were placed in the maxilla and 9 in the mandible.
Purpose: The aim of the present study was to evaluate the clinical outcome of extensive Empress onlays retained with resin-bonded cement.
Materials And Methods: One hundred thirty extensive ceramic onlays were placed in premolar and molar regions in 91 patients treated by 2 general practitioners between 1997 and 2000. Seventy-seven percent of the constructions were luted with chemically cured resin composite cement and 23% were luted with dual-cured resin cement.
Objective: Several studies have reported increased levels of gold (Au) in the blood of patients with dental gold restorations. This study analyzed gold levels in blood plasma before dental gold inlay insertion, 0-12 months after, and 15 years after.
Material And Methods: Plasma samples from 9 patients were taken before and 0-10 months after gold inlay insertion.
The aim was to evaluate the influence on the stress distribution patterns in and the magnitude of stresses on fixed partial dentures (FPDs) under different anatomic and design conditions. Three-dimensional finite element models of posterior 3-unit all-ceramic FPDs were created with and without periodontal ligaments, with different radii of curvature at the embrasure area, and in a curve shape with a periodontal ligament. The model with a periodontal ligament showed 40% higher stress values compared to the no-ligament model.
View Article and Find Full Text PDFActa Odontol Scand
August 2006
Objective: The purpose of this study was to evaluate the shear bond strength (SBS) of a dental luting agent to alumina ceramics after different surface pretreatment.
Material And Methods: Specimens (n=50) of pressed blocks (10 x 0 x 5 mm) of alumina ceramic (Procera AllCeram) were divided into untreated specimens (AF) as provided by the manufacturer and polished specimens (AP). Five groups of specimens (n=5 x 10) with different surface pretreatments were prepared.
Objectives: To evaluate the bond strength of dental resin agent to zirconia ceramic after surface pre-treatment with different techniques.
Methods: Specimens of hot isostatic pressed yttrium-oxide-partially-stabilized zirconia blocks (ZF) were fabricated (Procera Zircon, Nobel Biocare, Sweden) and compared to glossy dense zirconia blocks (ZG). Four groups of specimens with different surface treatment were prepared.
Objectives: Yttria-stabilized zirconia (Y-TZP) ceramic is a high-performance material with excellent mechanical properties suitable for fixed partial dentures. The purpose of this study was to evaluate after fatigue testing, the effect of heat-treatment and veneering on the fracture resistance of frameworks manufactured using sintered and subsequently hot isostatic pressed yttrium oxide partially-stabilized zirconia (Denzir).
Methods: The specimens were subjected to dynamic loading in water.
Purpose: The present follow-up study was carried out to evaluate the performance of Class II Cerec inlays after 10 years of clinical service.
Materials And Methods: Sixty-six Class II CAD/CAM ceramic inlays were placed in 27 patients. Each patient received at least one inlay luted with a dual-cured resin composite and one inlay luted with a chemically cured resin composite.
Purpose: The aim of this retrospective study was to investigate the longevity and clinical performance of fixed partial dentures (FPD) 30, 20, and 10 years after insertion.