Austenitic stainless steels are very popular due to their high strength properties, ductility, excellent corrosion resistance and work hardening. This paper presents the test results for joining AISI 316Ti austenitic steel. The technologies used for joining were the most popular welding techniques such as TIG (welding with a non-consumable electrode in the shield of inert gases), MIG (welding with a consumable electrode in the shield of inert gases) as well as high-energy EBW welding (Electron Beam Welding) and plasma PAW (plasma welding).
View Article and Find Full Text PDFThe paper concerns the effect of annealing time and temperature on the properties of the nitride layer on X37CrMoV51 tool steel used in the extrusion aluminium industry. Samples made from X37CrMoV51 steel were hardened and tempered, and then nitrided at 530 °C. After nitriding, the samples were annealed in a furnace at 470 °C for 8 h, 12 h, 24 h, 30 h and 60 h, and additionally for 20 h at 270 °C.
View Article and Find Full Text PDF