Aim: The aim of this study was to determine the sealing ability of three different materials mineral trioxide aggregate (MTA) Plus, bone cement, and calcium sulfate with self-etch adhesive (SEA) for the repair of furcal perforation, using dye extraction method.
Materials And Methods: Forty-eight extracted human permanent first and second molars were included and randomly divided into four groups: Group 1, n = 12, negative control, perforation not repaired with any material, Group 2, n = 12, perforation repair material used, MTA Plus, Group 3, n = 12, perforation repair material used, calcium sulfate with SEA, Group 4, n = 12, perforation repair material used, bone cement. The teeth were then coated with two coats of clear nail varnish immersed in methylene blue dye for 24 h, kept in 65% concentrated nitric acid for 3 days.