SiC-coated C/C composites with mechanical damage were repaired by the heat treatment method and slurry painting-preoxidation. The effects of different process parameters on the microstructure, interface bonding and oxidation resistance of Si-SiC repair coatings at 1773 K for 10 h were studied. The results show that the repair coating is tightly bonded to the original coating and the C/C substrate, and there is no obvious interface.