Objective: The aim of this in vitro study was to evaluate the influence of different finishing procedures on the wear behavior of zirconia against natural enamel.
Methods: 64 quadratic specimens (10 mm × 10 mm × 2 mm) were cut from a commercial hipped dental Y-TZP ceramic. Four different groups with 16 specimens each were formed according to the following finishing procedures: PZ (polished), RR (fine-grit diamond), GR (coarse-grit diamond), GZ (glazed).
Objectives: The aim of this study was to evaluate the mechanical properties and the subcritical crack growth behavior of a presintered dental Y-TZP (Kavo Everest ZS) and a hot isostatic pressed Y-TZP (Kavo Everest ZH) and to perform life data analysis.
Methods: For each material 150 bending bars were produced. The initial fracture strength was determined in a four-point bending test.