ACS Appl Mater Interfaces
November 2013
Porous graphitic carbon of high specific surface area of 1416 m(2) g(-1) and high pore volume of 1.11 cm(3) g(-1) is prepared by using commercial CaCO3 nanoparticles as template and sucrose as carbon source followed by 1200 °C high-temperature calcination. Sulfur/porous graphitic carbon composites with ultra high sulfur loading of 88.
View Article and Find Full Text PDFHierarchical micro/nanostructured MnO material is synthesized from a precursor of MnCO3 with olive shape that is obtained through a facile one-pot hydrothermal procedure. The hierarchical micro/nanostructured MnO is served as anode of lithium ion battery together with a cathode of spinel LiNi0.5Mn1.
View Article and Find Full Text PDF