Objectives: to evaluate the probability of survival and failure modes of lithium-disilicate, feldspathic-ceramic, and resin-nanoceramic anterior veneers cemented on dentin analog substrates after sliding-contact step-stress accelerated life testing (SSALT).
Methods: A virtual incisor tooth preparation was produced with a reduction of 1.5mm at the incisal edge and of 0.
Objective: To test the effects of different adhesive protocols and silane application on the adhesive durability to a Lithium Disilicate reinforced glass ceramic.
Methods: Forty disks of 13 mm diameter (E.max Press) were used.