J Nanosci Nanotechnol
February 2019
This study describes the electrodepositon of potentially competent oxygen evolution catalyst on inert anode using phosphate buffered solution containing cobalt ions. The thickness of deposited amorphous cobalt-phosphate catalyst thin film varies depending on the deposition potential and deposition time. The electrodeposited catalyst can actively be used to improve water oxidation reaction under neutral condition.
View Article and Find Full Text PDFJ Nanosci Nanotechnol
April 2017
Tungsten oxide thin film has been found great potential use in various applications such as smart window, gas sensor and photoelectrochemical cell due to their unique electrochromic, gas-chromic and electrochemical properties. The thin film morphology has been considered as an efficient limiting aspect for its performance. In this work, we successfully prepared tungsten oxide thin films with distinctive nanostructures on conductive glass in a flame vapor deposition process.
View Article and Find Full Text PDFVertically aligned nanostructured tungsten oxide thin films have been found useful in many applications due to its intrinsic photonic and electronic properties. In this study, we directly prepared vertically aligned nanostructures including nanowires and nanotubes grown directly on FTO-coated glass by a newly designed flame vapor deposition system. The deposition height was found to be an important parameter for the development of thin film morphology.
View Article and Find Full Text PDFJ Nanosci Nanotechnol
February 2016
Tungsten oxide thin films have been found as an active visible light driven photoanode material for photoelectrochemical water splitting due to its good stability in aqueous solution and energetically favorable valence band position for water oxidation. Morphology control, which determines the performance of WO3 photoanode, is one of most focuses of recent research interests. In this work, we successfully prepared monoclinic WO3 thin films on ITO glass at low range of substrate temperature with a fabrication rate around 100 nm per minute by using aerosol flame deposition process.
View Article and Find Full Text PDF