The electrical spark discharge method was used to prepare graphene copper nanocomposite (GNS-Cu) colloids under normal temperature and pressure. Cu and graphite were mixed in deionized water at a Cu : C mass ratio of 9 : 1 (99% purity), and the mixture was used to produce composite rods as the electrodes for spark machining. An electrical discharge machine with five settings of pulse cycle turn-on and turn-off times, namely 10-10, 30-30, 50-50, 70-70, and 90-90 μs, was used to prepare five different types of GNS-Cu colloids.
View Article and Find Full Text PDFThis study used an electrical discharge machine (EDM) to perform an electrical spark discharge method (ESDM), which is a new approach for reducing graphene oxide (GO) at normal temperature and pressure, without using chemical substances. A silver (Ag) electrode generates high temperature and high energy during gap discharge. Ag atoms and Ag nanoparticles (AgNP) are suspended in GO, and ionization generates charged Ag ions in the Ag plasma with a strong reducing property, thereby carrying O away from GO.
View Article and Find Full Text PDF