Six kinds of experimental magnetic resin composites containing SUS447J1 stainless steel particles as filler were prepared. UDMA/MAA resin with an MAA mole fraction of 0.67 was used as the matrix resin.
View Article and Find Full Text PDFNine kinds of experimental soft magnetic resin composites containing SUS447J1 stainless steel particles as filler were prepared. A UDMA/MAA resin with an MAA mole fraction of 0.67 was used as a matrix resin.
View Article and Find Full Text PDFA metal-resin composite material was experimentally prepared by mixing a powder consisting of Ag-Cu particles and BPO with a paste consisting of UDMA-based monomer and 4-META in the absence of tertiary amine. The working time and setting time were mainly affected by the amounts of 4-META, BPO and metal particles, most of them fulfilling the requirements for working time and setting time specified in ISO 4049:2000 in the present experimental conditions. The flexural strength ranged from 49.