This study investigated the effect of Er:YAG (smart 2940 Dplus, DEKA, Italy) and Er:CrYSGG (Waterlase iPlus, Biolase, USA) lasers on the shear bond strength (SBS) between the orthodontic brackets and dental porcelain in comparison with conventional acid etching with 9% hydrofluoric acid (HF, Ultradent, USA). A total of 60 specimens of maxillary incisor crown were prepared and randomly assigned to five groups; each group was subjected to a different porcelain surface conditioning: (1) etching with the 9% HF for 2 min; (2) etching with the 9% HF for 2 min followed by irradiation with the Er:CrYSGG laser (3-W power, 10-Hz frequency for 10 s); (3) etching with the 9% HF for 2 min followed by irradiation with the Er:YAG laser (3-W power, 10-Hz frequency for 10 s); (4) Irradiation with the Er:CrYSGG laser (3-W power, 10-Hz frequency for 10 s without acid etching) and (5) irradiation with the Er:YAG laser (3-W power,10-Hz frequency for 10 s without acid etching). After using Transbond XT primer and Transbond XT adhesive, the metal brackets (Dentaurum, Germany equilibrium 2, optimal design) bonded to the conditioned porcelain surface.
View Article and Find Full Text PDF