Objectives: This study evaluated the influence of the thickness of disilicate ceramic on the light attenuation (mW/cm2), degree of conversion (DC, %), Knoop hardness (KH, N/mm2) and the elastic modulus (E, MPa) of four luting resins.
Methods: Three resin cements: RelyX Veneer (RV, 3M Oral Care, Monrovia, CA USA); Allcem Veneer APS (AC, FGM); Variolink Esthetic LC (VE, Ivoclar Vivadent, Schaan, Liechtenstein) and one flowable resin composite Tetric N-Flow (TF, Ivoclar Vivadent) were photocured for 20 seconds. The irradiance (mW/cm2) and emission spectrum (mW/cm2/nm) from a broad-spectrum LED light unit (Bluephase G2, Ivoclar Vivadent) were measured over the luting material (control) and through 0.