When chord face failure occurs, one of the factors, which influence the resistance of the square hollow sections joint is the brace-to-chord width ratio of the joint. This includes the size of the weld connecting the two members. The influence of weld type and weld size on the behaviour of rectangular and square hollow section joints was studied at the Czech Technical University in Prague.
View Article and Find Full Text PDFFire exposure of timber leads to charring, surface cracking and timber burnout, shifting the external thermal load deeper into the timber domain. This phenomenon plays its role mainly in situations of longer fire exposure. The majority of current approaches and models assume initial geometry during the whole analysis, leading generally to the overestimation of the insulation effect of the charred layer and to a limited burnout.