Objective: The objective of this study was to evaluate the surface roughness (SR), water sorption (WS), and solubility (SO) of four composite resins after finishing/polishing and after one year of water storage.
Materials And Methods: Two low-shrinkage composites (Filtek Silorane [3M ESPE] and Aelite LS [Bisco Inc]) and two composites of conventional formulations (Heliomolar and Tetric N-Ceram [Ivoclar Vivadent]) were tested. Their respective finishing and polishing systems (Sof-Lex Discs, 3M ESPE; Finishing Discs Kit, Bisco Inc; and Astropol F, P, HP, Ivoclar Vivadent) were used according to the manufacturers' instructions.
Purpose: To evaluate the microshear bond strength of resin cements to yttrium-stabilized tetragonal zirconium oxide surfaces after water storage for 24 h or 1 year.
Materials And Methods: Four self-adhesive (BisCem, G-Cem, RelyX Unicem, SeT) and one conventional resin cement (RelyX ARC) were tested. The materials were mixed and inserted in tubes (0.
Objective: The purpose of this study was to evaluate the effects of the viscosities and curing modes on the degree of conversion (DC) of two resin cements.
Methods: Eight experimental groups were evaluated (n=5), according to the dual-cured resin cements (Nexus 2/Variolink II), viscosity (low and high) and evaluation time (5 minutes and 24 hours). The resin cements were applied to surface of a horizontal attenuated-total-reflectance unit and were polymerized either with self-cure (SC) or light exposure (XL3000/3M ESPE) for 40 seconds.
The purpose of this study was to evaluate the effects of adhesive primer applications on the bond strength of resin cements to cast titanium. Four adhesive primers - Metaltite, Metal Primer II, Alloy Primer and Ceramic Primer - and their respective resin cements - Bistite II DC, Link Max, Panavia F 2.0, RelyX Unicem and RelyX ARC - were tested.
View Article and Find Full Text PDFThe purpose of this study was to characterize the inorganic components and morphology of filler particles of conventional and self-adhesive, dual-curing, resin luting cements. The main components were identified by energy dispersive X-ray spectroscopy microanalysis (EDX), and filler particles were morphologically analyzed by scanning electron microscopy (SEM). Four resin cements were used in this study: two conventional resin cements (RelyX ARC/3M ESPE and Clearfil Esthetic Cement/Kuraray Medical) and two self-adhesive resin cements (RelyX Unicem/3M ESPE and Clearfil SA Luting/Kuraray Medical).
View Article and Find Full Text PDFThis study evaluated the effect of curing mode (auto- and dual-polymerizing mode) and time interval (5, 10 and 15 minutes) on the degree of conversion of resin cements. One conventional dual-cured resin cement (Panavia F 2.0 [Kuraray Medical Inc]) and two self-adhesive cements (RelyX Unicem [3M ESPE] and BisCem [BISCO, Inc]) were evaluated.
View Article and Find Full Text PDFJ Biomed Mater Res B Appl Biomater
April 2010
In this study, the in vitro bond strength of dual-curing resin cements to indirect composite restorations when the cement was either light polymerized or allowed to only autopolymerize was evaluated. Occlusal dentin surfaces of 56 extracted human third molars were flattened to expose coronal dentin. Teeth were assigned to eight groups (n = 7) according to resin cement products and polymerization modes: conventional cement (Panavia F 2.
View Article and Find Full Text PDFPurpose: The aim of this study was to evaluate the effectiveness of adhesive primers (APs) applied to Co-Cr and Ni-Cr metal alloys on the bond strength of resin cements to alloys.
Materials And Methods: Eight cementing systems were evaluated, consisting of four resin cements (Bistite II DC, LinkMax, Panavia F 2.0, RelyX Unicem) with or without their respective APs (Metaltite, Metal Primer II, Alloy Primer, Ceramic Primer).