The mixed material clay/Fe was prepared and immobilized on glass slides and calcined at 550 and 750 °C. The calcined material X-ray powder pattern (XRD) diffractograms indicate that there is no intercalation of iron compounds inside the lamella clay. The experimental design revealed that the most suitable phenol degradation conditions were obtained using the material calcined at 750 °C in a pH 7 and 140 mg/L of hydrogen peroxide solution.
View Article and Find Full Text PDFJ Colloid Interface Sci
September 2010
Akaganéite is a very rare iron oxyhydroxide in nature. It can be obtained by many synthetic routes, but thermohydrolysis is the most common method reported in the literature. In this work, akaganéite-like materials were prepared through the thermohydrolysis of FeCl(3).