Purpose: To investigate the impact of printing layer thickness on the optical properties and surface roughness of various 3D-printed resins manufactured by digital light processing (DLP) and indicated for provisional and definitive restorations.
Materials And Methods: A total of 240 specimens from four different 3D-printing resins-VarseoSmile Crown Plus (Bego; VS), Crowntec (Saremco Dental; CR), GC Temp PRINT (GC Dental; TG), and NextDent C&B MFH (NextDent; ND)-were divided into four groups (n = 60 per group). Each group was further divided into three subgroups (n = 20) according to printing layer thickness (25, 50, and 100 μm).