This study verifies whether there is any temperature change during photoactivation of two resin composites (Filtek Z250 and Filtek Flow) with three different light curing methods (conventional halogen light curing unit, light emitting diodes curing unit and xenon plasma arc curing unit) and the relationship of temperature change with resin composite hardness. A type-K thermocouple registered the temperature rise peak in an elastomer mold during photoactivation. After photoactivation, the specimens were submitted to Knoop hardness test performed by an indenter (HMV-2000) under a load of 50g for 15 seconds.
View Article and Find Full Text PDFThe relationship between the application of die-spacer prior to wax pattern fabrication and metal removal from the inner surface of the casting on marginal and internal discrepancies of complete cast crowns was evaluated. One hundred and twenty complete crowns were cast with palladium-silver alloy melted by gas-oxygen torch or electrical resistance and cast with a centrifuge casting machine. After casting, the crowns were seated on each type of different marginal configuration dies (90-degree shoulder, 20-degree beveled shoulder, and 45-degree chamfered shoulder) with a static load of 90 N during 1 min.
View Article and Find Full Text PDF