The present work was carried out on Al-7%Si-0.4%Mg-X alloy (where X = Mg, Fe, Sr or Be), where the effect of solidification rate on the eutectic silicon characteristics was investigated. Two solidification rates corresponding to dendrite arm spacings (DAS) of 24 and 65 μm were employed.
View Article and Find Full Text PDFThe present study was performed on A356 alloy [Al-7 wt %Si 0.0.35 wt %Mg].
View Article and Find Full Text PDF