The aim of this study is to investigate the repair bond strength of composite resin following three different surface treatments (bur-grinding, silanization, and Er,Cr:YSGG laser irradiation) using various universal adhesives. A total of 160 resin composite specimens, produced in cylindrical form (6 × 2 mm) with a nanohybrid composite resin within metal molds, were subjected to 5000 cycles of aging in a thermocycler. The aged samples were categorized into four groups based on surface treatments: control, bur, silane, and Er,Cr:YSGG laser.