We describe a process for fabricating a wafer-scale array of alkali metal vapor cells with low residual gas pressure. We show that by etching long, thin channels between the cells on the Si wafer surface, the residual gas pressure in the evacuated vapor cell can be reduced to below 0.5 kPa (4 Torr) with a yield above 50%.