The present study aims to see the enhancement in thermoelectric properties of bismuth telluride (BiTe) annealed at different temperatures (573 and 773 K) through silver (Ag) nano-inclusions (0, 2, 5, 10, 15 and 20 wt %). Transmission electron microscopy (TEM) images of Ag incorporated in BiTe annealed at 573 K shows tubular, pentagonal, trigonal, circular and hexagonal nanoparticles with sizes of 6-25 nm (for 5 wt % Ag ) and 7-30 nm (for 20 wt % Ag). Ag incorporated in BiTe annealed at 773 K shows mainly hexagonally shaped structures with particle sizes of 2-20 nm and 40-80 nm (for 5 wt % Ag) and 10-60 nm (for 20 wt % Ag).