Objectives: To examine the micro tensile bond strength (μTBS) and the resin-dentin interface on a laser-irradiated dentin surface using two different irradiation methods, with or without additional low-energy irradiation.
Methods: The flat bovine dentin surface was divided into three groups: i). control group (C group, no irradiation), ii) 80 mJ/pulse Er: YAG laser group (80 group), iii) 80 + 30 mJ/pulse Er: YAG laser group (80 + 30 group, with an additional 30 mJ/pulse).