Aim: The aim of this study was to investigate the association of different degradations on the roughness, gloss, and color changes of microhybrid composites.
Materials And Methods: Ten specimens were prepared for Charisma, Amelogen Plus, Point 4, and Opallis resins. Surfaces were polished and baseline measurements of roughness, gloss, and color were recorded.
The aim of this study was to evaluate the shear bond strength of resin composite repairs with and without aging of the surface to be repaired, using different adhesive systems and resin composites. Ninety specimens were prepared: 10 for the Control Group (GC - without repair); 40 for Group I (GI - repairs after 7 days) and 40 for Group II (GII - repairs after 180 days). Groups I and II were divided into 4 subgroups of 10 specimens each, according to the adhesive system and composite resin used: A) Adper Scotch Bond Multipurpose + Filtek Z350 XT; B) Adper Single Bond Plus + Filtek Z350 XT; C) Adper Scotch Bond Multipurpose + Esthet-X; D) Adper Single Bond Plus + Esthet-X.