This research analyzed the effect of the manufacturing method on the flexural strength and color stability of 3D-printed resins used for producing indirect restorations. For this, two dental restorative biocompatible resin materials, OnX (OnX, SprintRay) and CB (Crown and Bridge, Dentca), were divided into 2 groups according with manufacturing method (printed with a Pro95 3D printer - SprintRay; and not printed, with samples obtained with the fluid resin being poured on PVS molds for further light activation in the post-curing process), and subdivided into 2 groups according to the post-curing method: VG (Valo Grand, Ultradent Products) for 120 s and PC (Procure 2, SprintRay). Bar-shaped samples were used to evaluate the flexural strength 24 h after storage in distilled water at 37 °C using a universal testing machine.