Silicon is expected to become the ideal anode material for the next generation of high energy density lithium battery because of its high theoretical capacity (4200 mAh g ). However, for silicon electrodes, the initial coulombic efficiency (ICE) is low and the volume of the electrode changes by over 300% after lithiation. The capacity of the silicon electrode decreases rapidly during cycling, hindering the practical application.