Purpose: This study evaluated the shear bond strength (SBS) of resin cement to dentin after applying two adhesive (A) systems with a combination of four different immediate dentin sealing (IDS) strategies, and two surface conditioning (SC) methods.
Material And Methods: Human third molars (n = 140) were collected and randomly split (n = 70 each) between the two A systems (Clearfil SE Bond; Kuraray [AC] and Optibond FL; Kerr [AO]). The A groups were further divided into four IDS strategies (2 x one adhesive layer (IDS-1L); 2 x two adhesive layers (IDS-2L); 2 x one adhesive layer and one flowable layer (IDS-F); 2 x no adhesive layer (delayed dentin sealing [DDS]).