For this study, 120 fragments obtained from human third molars were randomly separated into 12 groups (n = 10). Four groups were used for measuring the Knoop hardness number (KHN) of enamel, while the other eight were used for testing the microtensile bond strength (muTBS) of two adhesive systems (Single Bond and Prime & Bond NT). All groups presented statistically similar KHN values.