To solve the problem of vascular access failure, a novel semi-degradable hybrid vascular graft, manufactured by electrospinning using silk fibroin and polyurethane (Silkothane), has been previously developed and characterized in vitro. This proof-of-concept animal study aims at evaluating the performances of Silkothane grafts in a sheep model of arteriovenous shunt, in terms of patency and short-term remodeling. Nine Silkothane grafts are implanted between the common carotid artery and the external jugular vein of nine sheep, examined by palpation three times per week, by echo-color Doppler every two weeks, and euthanized at 30, 60, and 90 days (N = 3 per group).