Osteoconductive bioglasses, free of K(2)O and Al(2)O(3) and with content of Na(2)O lower than 10 mol%, were designed based on the ratio (SiO(2) + MgO)/(P(2)O(5) + CaO + Na(2)O) in the system Na(2)O-CaO-MgO-P(2)O(5)-SiO(2). The developed glasses have shown a strong potential for the formation of hydroxycarbonated apatite (HCA) in vitro. The particles of HCA aggregates tend to be of finer size with increasing the ratio of (SiO(2) + MgO)/(CaO + P(2)O(5) + Na(2)O) in the glass chemical composition indicating significant bioactivity.